Slag film flowing of cyclone burner is analyzed in this paper and the solution equa- tion set for slag film thickness is presented.
对液态排渣旋风燃烧器的渣膜流动进行分析,给出渣膜厚度的求解方程组,并对定性分析渣膜厚度对传热的影响,为液态排渣燃烧器的结构设计、耐火材料的选择与修补提供切实可行的实施手段。
2.
An experimental apparatus for simulating copper mold was used to quantify the heat flux density through the slag film of mould flux,and a solid slag was obtain for further studying the influence of slag film microstructure on heat flux density by microscope, scanning electron microscope and X-ray diffraction.
针对由CaO-SiO_2-CaF_2-Na_2O组成的四元渣系,采用模拟铜结晶器实验装置制取固态渣膜,实现结晶器保护渣渣膜水平传热的定量化研究。
3.
Heat flux of slag film in mold was simulated in the laboratory by a homemade device which can quantify the heat flux and acquire the slag film.
利用本实验室开发出的一套渣膜热流模拟测试装置,完成渣膜热流的定量化测试及渣膜的制取。
2)  flux film
渣膜
1.
The flux film between mold and billet directly affects the heat transfer and lubrication of the billet,because F-free mold powder differs from the traditional powder,the characters and its heat behavior are the key to the development of F-free mold powder.
结晶器和铸坯间的渣膜直接影响铸坯的润滑和传热,由于无氟保护渣特性不同于传统含氟渣,其传热特性以及它在结晶器内的热行为是研发的关键。
2.
The present paper studied the solidified film structure,mineralogical compositions and crystallizing-out rate of the mould flux for the thin slab continuous casting and analyzed the effect of the structure of the solidified flux film on the heat transfer of the slab as well as the proper way to improve the surface quality of the slab by controlling the solidified microstructure of the flux film.
研究了薄板坯连铸结晶器保护渣渣膜的凝固组织结构、矿相组成、析晶率,分析了固态渣膜结构对铸坯传热的影响以及通过控制渣膜凝固结构提高连铸表面质量的途径。
3.
A simulated appartus is designed for measuring the heat transfer through the layer of continuouns casting flux between the mold and the solidified shell,and it is used to study the heat transfer behavior of flux film in the continuous casting mold.
用自制的一台模拟试验装置研究了连铸结晶器中渣膜的热传导行为。
3)  slag film
渣皮,渣膜
4)  flux film
保护渣膜
5)  Solidified Flux Film
固态渣膜
1.
The solidified flux film of mould powder for beam blank of Nb micro-alloyed medium carbon steel was studied by optical microscope, scanning electron microscope and X-ray diffraction analysis.
利用光学显微镜、扫描电镜(SEM)和X射线衍射仪(XRD),对用于浇铸含Nb中碳钢异型坯的试验保护渣固态渣膜进行了分析。
6)  film phases
渣膜矿相
1.
The composition of flux effect film phases and erforrnance directly,whether flux suit to produce of casting, the key is whether composition is fit,so it is important that research on influence of composition of mould flux for casting on phases and performance.
保护渣的组成直接影响渣膜矿相及其性能,保护渣是否适应连铸生产,关键在于保护渣是否有适宜的组成,所以,研究保护渣的组成对渣膜矿相以及性能的影响对铸坯质量的改善有重要意义。