1)  mesoporous zirconia
介孔氧化锆
1.
Palladium oxide and/or ceria can be successfully incorporated into mesoporous zirconia via a surfactant assisted method with a suitable post-treatment process.
利用表面活性剂辅助模板及适当后处理工艺实现了少量贵金属氧化钯及稀土氧化铈在有序介孔氧化锆孔道中或孔道表面的均匀分散/负载。
2.
A steady mesoporous zirconia nanocrystallite has been successfully synthesized by the anionic surfactant-assisted route.
利用阴离子表面活性剂十二烷基磺酸钠(SDS)为辅助模板剂,成功地合成了高稳定性的介孔氧化锆纳米晶,采用DSC-FG,FT-IR,XRD,TEM,UV-Vis以及N2吸附-脱附等方法对样品进行了表征。
3.
In this paper, yttrium can be successfully incorporated into the framework of mesoporous zirconia by a surfactant-assisted method and a post-treatment process.
作者利用表面活性剂辅助模板及后处理工艺成功实现了过渡金属钇在有序介孔氧化锆骨架中的掺杂改性 。
2)  mesoporous zirconia
介孔二氧化锆
1.
In this paper, by using different surfactants, mesoporous alumina and mesoporous zirconia are prepared through the co-assembly of block copolymer and inorganic sol-gel process, then rare earth ions are introduced into mesoporous alumina and zirconia to prepare luminescent materials.
第五章、第六章仿照前述方法制备介孔二氧化锆及组装其发光物质。
3)  mesoporous zirconia film
介孔氧化锆膜
4)  porous zirconium oxide
多孔氧化锆
1.
Many researches have been focused on the synthesis of ordered porous zirconium oxide in the world.
有序多孔氧化锆是近年来国际上的研究热点之一,本文利用表面活性剂辅助模板机 理成功地合成出稳定性高(>550℃)、比表面积大(>350m2/g)、且有序度高的多孔氧化锆, 并用FT-IR、XRD、HRTEM,以及N2吸附-脱附等方法进行了表征。
5)  ordered porous zirconium oxide
有序多孔氧化锆
6)  mesoporous silica
介孔氧化硅
1.
Organo-functionalized mesoporous silica has great potentials in practical applications such as catalysis,adsorption and separation,biochemistry and electronics.
有机功能化的介孔氧化硅在催化领域、吸附分离、生物化学和电子学等领域有广泛的应用前景。
2.
The structure of mesoporous silica before and after functionalization was investigated by high-resolution transmission electron microscopy(HRTEM),fourier transfor.
采用直接模板法,以三嵌段共聚物P123作为模板剂,酸性条件下制备出了具有规则孔道结构的介孔氧化硅。
3.
The mesoporous silica material (SH), with controlled pore size has been synthesized using hexadecyltriethylammon um bromide (CTAB) as template under acidic condition at room temperature.
以十六烷基三甲基溴化铵作模板剂,采用酸性常温法制备介孔氧化硅材料SH,通过添加TMB扩孔剂对其进行改性得到SH+TMB,分别测试其吸湿、放湿性能,并采用小角度XRD、TEM、B。
补充资料:氧化锆-氧化钇红外陶瓷
分子式:  ZrO2-Y2O3 
CAS号:

性质:一种以二氧化锆为基体固溶6%~8%(mol)氧化钇的红外光学材料。立方晶结构。熔点2700℃。密度5.98g/cm3。红外透射波段1~10μm。采用1450℃以上高温烧结或1300~1700℃,50~300MPa热压制取。用于制造耐高温红外窗口和整流罩。