1)  Rupture life
断裂寿命
1.
The effects of temperature and applied stress on rupture life, and the relations of temperature, applied stress and rupture life to characteristic dimensions of coherent phases (γ matrix channel width and rafted γ precipitate thickness), and to the elongation as well as to the cross sectional area reduction of the tested specimens were investigated.
在 760-1050℃和780-115 MPa范围内,选择不同温度和应力配合进行了持久拉伸实验,研究了温度和应力的变化对试件断裂寿命的影响以及温度、应力和断裂寿命与共格相特征尺寸(基体相γ水平通道宽度、筏形析出相γ厚度)和试件延伸率及断面收缩率的关系。
2.
The P92 steel is a steel sort being used for main steam pipelines of ultra-supercritical units at present,its creep rupture life has widely drawn close attention.
P92钢是目前超超临界机组主蒸汽管道的应用钢种,其蠕变断裂寿命被广泛关注。
2)  creep rupture life
蠕变断裂寿命
1.
In this paper the effect of Ce-La mixed RE content and environment conditions on the creep rupture life of Sn2.
7CuxRE钎料钎焊接头蠕变断裂寿命的影响。
2.
Based on an advanced neural network method and a huge number of creep rupture life data of nickel base single crystal superalloys, an artificial neural network model is constructed to predict creep rupture life for different types of nickel-base single crystal superalloys.
根据大量镍基单晶高温合金在不同温度和应力下的蠕变断裂寿命数据,采用一种先进的人工神经网络方法建立运算模型,对合金在不同实验或运行条件下的蠕变断裂寿命进行了预测,并将测算结果与现有其它方法进行了比较。
3.
Based on experimental data, an artificial neural network method is used to develop a model to predict the creep rupture life of different types of nickel-base wrought superalloys.
在试验数据的基础上,利用人工神经网络建立不同成分镍基变形合金的不同温度,外应力与蠕变断裂寿命之间关系模型,并进行网络训练,对合金的蠕变断裂寿命进行模拟。
3)  creep-rupture life
蠕变断裂寿命
1.
The results indicate that proper quantities of Ce can remarkably prolong the creep-rupture life of the Sn3Ag2.
8Cu钎焊接头在室温下的蠕变断裂寿命,Sn3Ag2。
4)  FCI life
始裂寿命
5)  rupture life
破裂寿命
6)  life diagnosis
寿命诊断
1.
,and combining the features in China,the theory system on life diagnosis is put forward for the important hydraulic engineerings.
针对重大水利水电工程中存在的严重隐患缺陷或丧失功能,吸收美国等对此处理的先进理论和方法,并结合我国的特点,构建了重大水利水电工程寿命诊断的理论体系,并提出了水利水电工程生存寿命的原则,即安全原则、工程效益原则以及生态环境原则。
2.
The measures that life diagnosis of reheater by the thickness-detecting technology for oxide-scale on inner-side of tube, the increase of tube temperature detecting p.
结合莱城电厂2号锅炉末级再热器超温爆管实例介绍了采用内壁氧化皮测厚技术进行再热器寿命诊断、增加管屏壁温测点及开发壁温监测系统的处理措施。
补充资料:百二十岁寿命
【百二十岁寿命】
 (传说)据经论所说,释尊出世,人寿百岁之时也。智度论四曰:“人寿百岁,佛出时到。”弥勒上生经疏上曰:“释迦减劫百岁出世,弥勒增劫出世。”然佛寿有二说:一人寿百岁之时,则佛寿亦百岁。为以其福分与未来之弟子,减寿之第五分(五分百岁也),八十入灭。二人寿百岁,而佛过于众人,其寿命亦超过之,为百二十岁。只为末世之弟子,减第三分(三分百二十岁),八十入灭。大集月藏经第十法灭尽品曰:“我今为众生弃舍身寿命,为增三精气,悲愍众生故,舍身寿第三分,令我法海满,洗浴诸天人。”大毗婆沙论百二十六曰:“有作是说:诸佛世尊舍第五分寿。有作是说:诸佛世尊舍第三分寿。若说诸佛舍第三寿者释迦牟尼佛寿量应住百二十岁,舍后四十但受八十。(中略)若说诸佛舍第五寿者,释迦牟尼世尊所感寿量应住百岁。舍后二十,但受八十。”