1) residual wall thickness
![点击朗读](/dictall/images/read.gif)
残余壁厚
2) residual wall thickness
![点击朗读](/dictall/images/read.gif)
残留壁厚
1.
The effects of the processing parameters on the water penetration length and residual wall thickness along water channel of polypropylene curved pipes molded by short shot water-assisted injection molding were investigated through single factor experiments.
介绍了自主研发的水辅助注塑设备以及一款经过大量实验后得到的新型喷嘴,并通过单因素实验法研究了短射法成型聚丙烯弯管时工艺参数对制品水穿透长度和沿水道的残留壁厚的影响。
2.
The recent contribution on water assisted injection technology is sumed up,including the flow behavior of polymer melt,the influence of processing parameters on the residual wall thickness and water penetration length,micro-morphology and mechanical properties,numerical simulation technology,etc.
水辅助注塑是在气体辅助注塑基础上发展起来的一种成型中空制品的新技术,综述了水辅助注塑中熔体的流动行为、工艺参数对制品残留壁厚及穿透长度的影响、制品微观形态及力学性能和数值模拟技术的最新进展,最后对水辅助注塑技术研究前景进行展望。
3) Residual thickness
![点击朗读](/dictall/images/read.gif)
残余厚度
4) remaining thickness
![点击朗读](/dictall/images/read.gif)
剩余壁厚
5) thin wall welded structure residual stress
![点击朗读](/dictall/images/read.gif)
薄壁结构残余应力
6) allowed minimum residual wall thickness
![点击朗读](/dictall/images/read.gif)
允许最小剩余壁厚
补充资料:凹模壁厚及凹模垫板尺寸
型腔壁部投影面积 壁 厚, 毫 米
F, 厘米2 h1 h2 h3 h4 h5
<5 15~20 30~40 <=10 15~20 30~40
>5~10 20~25 40~50 10~15 20~25 40~55
>10~50 20~30 50~60 15~20 20~30 55~65
>50~100 30~35 60~75 20~25 30~40 65~70
>100~200 35~40 75~85 25~30 40~50 70~75
>200 >40 >85 30~35 50~60 >80
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条