1) Fe-C-Si-Mn alloys
Fe-C-Si-Mn合金
1.
Fe-C-Si-Mn alloys are used as blades in hydroelectric generators contained network structures af- ter some heat treatments.
水轮机叶片用Fe-C-Si-Mn合金铸钢热处理后存在网状组织。
2) Fe-Mn-Si-Ni-C shape memory alloy
Fe-Mn-Si-Ni-C合金
3) Fe-Mn-Ni-C-Si alloy
Fe-Mn-Ni-C-Si合金
4) Fe-Ni-Mn-C-Si alloy
Fe-Ni-Mn-C-Si合金
5) Fe-Mn-Si-C shape memory alloy
Fe-Mn-Si-C形状记忆合金
1.
This paper discussed the effect of pre-deformation and mechanical training on the restoring ratio of Fe-Mn-Si-C shape memory alloy(SMA) which was produced in normal atmosphere by virtue of salvaged steel and pig iron with special protectant, of which the memory effect is achieved by stress-induced martensitic phase transformation.
利用废钢和生铁为原料,采用特殊保护剂,在大气中熔炼出Fe-Mn-Si-C形状记忆合金;利用应力诱发马氏体相变对Fe-Mn-Si-C合金实现形状记忆效应,探讨了预变形量和机械训练对Fe-Mn-Si-C合金回复率的影响规律。
6) Fe-18Cr-Mn-C-Mo(Si)-N system
Fe-18Cr-Mn-C-Mo(Si)-N合金系
补充资料:Fe-Si alloy
分子式:
CAS号:
性质:含硅0.5%~4.5%的铁硅合金。为硅在铁中的置换固溶体,属立方晶系。饱和磁感应强度为1.6~1.9J,铁损1~8W/kg。除了冲片使用外,常做成薄带,卷绕成铁芯。采用冷轧或进而热处理的方法获取结构(晶粒定向排列)。电力工业中用于电机、变压器等。电子工业中主要用于电源变压器、磁放大器等。
CAS号:
性质:含硅0.5%~4.5%的铁硅合金。为硅在铁中的置换固溶体,属立方晶系。饱和磁感应强度为1.6~1.9J,铁损1~8W/kg。除了冲片使用外,常做成薄带,卷绕成铁芯。采用冷轧或进而热处理的方法获取结构(晶粒定向排列)。电力工业中用于电机、变压器等。电子工业中主要用于电源变压器、磁放大器等。