Corrosion resistance,adhesion,porosity and hydrogen embrittlement of Zn-Fe-SiO_2 composite coatings with different thickness have been tested systematically,and these data have been compared with the properties of Zn and Zn-Fe alloy.
分别采用硫酸盐体系和氯化物体系的最佳工艺条件电沉积制备了高铁(Fe mass%>1%)和低铁(Fe mass%<1%)的Zn-Fe-SiO2复合镀层,并系统测试了不同厚度Zn-Fe-SiO2复合镀层的耐蚀性、结合力、孔隙率和氢脆性等综合性能,同时与电镀Zn及Zn-Fe合金进行了对比。
2.
Corrosion resistance, adhesion, porosity and hydrogen embrittlement of Zn-Fe-SiO2 composite coatings were tested systematically, and these data was compared with the properties of Zn and Zn-Fe alloy.
分别采用硫酸盐体系和氯化物体系的最佳工艺条件电沉积制备了高铁(Femass%>1%)和低铁(Femass%<1%)的Zn-Fe-SiO2复合镀层,并系统测试了不同厚度Zn-Fe-SiO2复合镀层的耐蚀性、结合力、孔隙率和氢脆性等综合性能,同时与电镀Zn及Zn-Fe合金进行了对比。
2)  hydrogen brittleness
氢脆性,氢脆
3)  hydrogen embrittlement
氢脆性,氢脆,氢脆变
4)  hydrogen embrittlement
氢脆性,氢脆化
5)  hydrogen embrittleness
氢蚀脆性
6)  hydrogen induced embrittlement
氢致脆性
补充资料:冲击脆性试验
分子式:
CAS号:

性质:在一定温度下对固定的试片给予一定的冲击,以观察试片破坏或龟裂等异状的试验,是评价材料抵抗冲击能力或判定材料脆性或韧性的重要试验方法。常见的冲击试验有摆锤式、落球式和高速拉伸冲击试验等。高分子材料的抗冲击性受温度、湿度、冲击速度、几何形状、材料历史以及应力方式等诸多因素的影响。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条