说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 倾倒-弯曲
1)  slanting-benting
倾倒-弯曲
2)  crooked-toppling
弯曲-倾倒
3)  flexural toppling
弯曲倾倒
1.
It is clear that the flexural toppling behavior is influenced by the geological structure significantly,and the numerical method based on continuum theory does not seem to work well.
弯曲倾倒是其中的一种特殊破坏形式,这种形式的边坡破坏和地质构造有很大的关系,用通常的连续介质理论不能很好地模拟和解析。
4)  bending-pull-type
倾倒弯曲-拉裂
5)  bending-dumping damage
弯曲倾倒破坏
1.
Pointing at the landslide resulted from the rainfall and taking the anti-dip rock slope as example,a simple bending-cracking model of mechanics is established based on the mechanical analyses of anti-dip rock layers,and the mechanism about the bending-dumping damage of this slope is analyzed by using the catastrophic theory.
针对降雨触发的滑坡,以反倾岩质边坡为例,在岩层受力分析的基础上,提出了一个简单的力学模型,并运用突变理论分析该类边坡弯曲倾倒破坏的力学机制。
6)  Bending and toppling deformation
弯曲倾倒变形
补充资料:弯曲工艺的概念及弯曲件

1.弯曲工艺:是根据零件形状的需要,通过模具和压力机把毛坯弯成一定角度,一定形状工件的冲压工艺方法。


2.弯曲成形工艺在工业生产中的应用:应用相当广泛,如汽车上很多履盖件,小汽车的柜架构件,摩托车上把柄,脚支架,单车上的支架构件,把柄,小的如门扣,夹子(铁夹)等。 


弯曲的基本原理:以V形板料弯曲件的弯曲变形为例进行说明。其过程为: 
   1. 凸模运动接触板料(毛坯)由于凸,凹模不同的接触点力作用而产生弯矩, 在弯矩作用下发生弹性变形,产生弯曲。
  2. 随着凸模继续下行,毛坯与凹模表面逐渐靠近接触,使弯曲半径及弯曲力臂均随之减少,毛坯与凹模接触点由凹模两肩移到凹模两斜面上。(塑变开始阶段)。
  3.随着凸模的继续下行,毛坯两端接触凸模斜面开始弯曲。(回弯曲阶段)。
   4.压平阶段,随着凸凹模间的间隙不断变小,板料在凸凹模间被压平。
  5. 校正阶段,当行程终了,对板料进行校正,使其圆角直边与凸模全部贴合而成所需的形状。 


弯曲变形的特点:  弯曲变形的特点是:板料在弯曲变形区内的曲率发生变化,即
弯 曲半径发生变化。从弯曲断面可划分为三个区:拉伸区、压缩区和中性层。