1)  morphology of corrosive pore distribution
蚀孔形貌
2)  corrosion morphology
腐蚀形貌
1.
5% NaCl solution was studied by static corrosion tests,corrosion rate calculation and corrosion morphology observation.
为了改善镁合金的耐腐蚀性能,进一步拓宽镁合金的应用范围,利用静态腐蚀试验,辅以腐蚀速率计算和腐蚀形貌观察,研究了混合稀土对镁合金AZ81在3。
2.
The theory of fractal geometry is used to analyze the corrosion morphology images, which were acquired by scanner.
将分形的概念应用于腐蚀形貌图像的特征提取,计算扫描得到的实海腐蚀试片图像的分形维数、广义维数、面积因子和空隙特征,并作为分析诊断系统的输入,用模糊模式识别理论建立了基于图像分形特征的腐蚀形貌图像诊断系统,可以由图像的分形特征值判断金属的表面腐蚀形貌。
3.
The system comprises three major modules:database and management system,corrosion prediction and corrosion morphology analysis.
采用面向对象的编程语言VisualBasic(VB)编制了金属材料海洋环境腐蚀数据咨询管理和预测诊断系统 ,系统中包含常用金属材料实海腐蚀数据和腐蚀形貌图谱的图文数据库 。
3)  pit morphology
点蚀形貌
1.
?The pit morphology of SiCp/2024 Al metal matrix composites (MMCs) in 3.
用扫描电镜对浸泡在w(NaCl)=3 5%水溶液中的SiCp/2024Al金属基复合材料(AlMMCs)的点蚀形貌进行了观察,作为对比,对其基体合金的点蚀行为也进行了研究·结果表明,SiCp/2024AlMMCs的点蚀形貌与SiC颗粒的体积分数和尺寸有关,SiC含量高或尺寸小的AlMMCs,其蚀孔数量较多,尺寸较小·与基体合金相比,AlMMCs的点蚀孔较大,数量较少,分布也较不均匀,甚至出现局部严重腐蚀的现象·能谱分析表明,SiCp/2024AlMMCs的腐蚀机制为富Cu阴极相与贫Cu阳极相间的电偶腐蚀·另外,SiC与Al间也存在电偶腐蚀倾向
4)  pore morphology
孔隙形貌
1.
The influence of the particle size of raw powders on the sintered properties such as sintered density, pore morphology, metallographic structure and mechanical properties were investigated.
25μm的3种较粗(相对于一般注射成形用细粉而言)水雾化316L不锈钢粉末进行了注射成形, 讨论了粉末粒度对金属注射成形烧结件性能, 如烧结密度、孔隙形貌、金相组织和力学性能的影响。
5)  keyhole profile
小孔形貌
1.
According to laser deep penetration welding existing the characteristics of keyhole,create a micron-size precise calculation model that coincidence with the keyhole profile.
根据激光深熔焊存在小孔现象的特点,利用符合小孔形貌特点的高斯旋转曲面体热源进行加载,得到了随激光工艺参数改变而变化的小孔形貌。
2.
Using the Gaussian rotating curved body heat source fitting for the keyhole profile and combining the material property of TC4 titanium alloy, the distribution characteristics of keyhole profile and transient welding temperature varying with the laser parameters have obtained.
结合TC4钛合金材料属性,利用能量分布与小孔形貌特点相类似的高斯旋转曲面体热源进行加载,得到了随激光焊接工艺参数改变而变化的小孔形貌及瞬态温度分布特征。
6)  dissolved micro-shape
溶蚀微形貌
1.
In this paper,dissolved micro-shape and stress micro-shape of the quartz,which were collected from the gouge of the Nalinlaka fault,Lhasa,Tibet,are observed and statistically analysed by ESEM.
利用环境扫描电镜,对西藏拉萨那林拉卡断裂白定段断层泥石英样品进行了溶蚀微形貌统计分析及应力痕迹微形貌观察。
补充资料:孔蚀
分子式:
CAS号:

性质:又称坑蚀,斑点腐蚀,小孔腐蚀或点蚀。金属表面大部分区域腐蚀相对较轻,而某些局部出现向纵深发展的腐蚀小孔的腐蚀形态。孔蚀的原因是活性阴离子导致表面钝化膜局部破坏。具有钝化能力的金属如不锈钢、铝合金及碳钢等,在含氯离子介质中经常发生孔蚀。蚀孔的发展速度有时很快,可以深入金属甚至短时间内蚀穿金属截面,且较难预测,因此孔蚀往往比均匀腐蚀具有更大的危害性。可以通过降低介质中的有害阴离子浓度,采用涂层保护、添加缓蚀剂和阴极保护等方法予以减轻或防止。