1) laminates/thermal postbuckling
层板/热后屈曲
2) thermal post-buckling
热后屈曲
1.
The thermal post-buckling behaviors of FGM rod made of ZrO-2 and Ti-6A1-4V were analyzed by shooting method.
对两端不可移简支陶瓷-金属功能梯度材料(FGM)杆建立了在热载荷作用下的非线性控制微分方程,采用打靶法分析了由二氧化锆和Ti-6Al-4V两种材料组成的FGM杆的热后屈曲行为。
3) thermal postbuckling
热后屈曲
1.
The thermal postbuckling of circular plate has been investigated by using Ritz method.
用Ritz法对各向同性圆板在周边转动弹性约束下的热后屈曲进行了研究。
2.
A thermal postbuckling analysis is presented for a rectangular plate subjected to uniform and nonuniform (parabolic) temperature loading and resting on a "softening" nonlinear elastic foundation.
采用摄动——Galerkin混合法给出完善和非完善矩形板热屈曲载荷和热后屈曲平衡路径。
3.
A thermal postbuckling analysis is presented for a rectangular plate subjected to uniform and nonuniform (parabolic)temperature loading.
采用摄动-Galerkin混合法给出完善和非完善矩形板热屈曲载荷和热后屈曲平衡路径。
4) laminate/delamination buckling
层合板/脱层屈曲
5) Buckling/Post-Buckling
屈曲/后屈曲
6) BucklingPostbuckling
屈曲后屈曲
补充资料:N,N-二缩水甘油2,4,6-三溴苯胺玻璃布层合板
分子式:
CAS号:
性质:以三溴苯胺环氧树脂为基料的玻璃布层合板。耐燃性好,相对密度>1.98。机械强度除冲击强度(190kJ/m2)和剪切强度(119MPa)外,其他略次于E-51环氧树脂。将三溴苯胺环氧树脂与有关添加剂配成胶液后,手工糊于玻璃布上,叠层并层合固化即得。可用于要求耐燃的航空、船舶和机电行业。