In our country, no-bake furan resin is one of the main molding materials in the production of cast-iron products, low nitrogen furan resin is also abroad used in the production of cast-Steel products, at present, it is one of the widest applications in foundry binders at home.
自硬呋喃树脂是我国铸造行业中铸铁件所使用的主要造型(芯)材料,同时对于低氮的呋喃树脂来说也广泛用于铸钢件的造型材料中,呋喃树脂是我国在造型材料中应用最多的树脂砂之一,但呋喃树脂在生产及制备砂型方面还存在着一些问题,主要表现在:树脂粘结剂含氮量偏高,砂型固化速度慢,生产效率不高,树脂粘结剂成本较高,合成树脂中游离甲醛含量偏高,致使在混砂、造型和浇注过程中散发有害气体,污染环境,损害工人身体健康。
2)  the furan resin grit
呋喃树脂自硬砂
1.
We analyzed the reason why the ordinary clay molding sand is replaced by the furan resin grit.
介绍呋喃树脂自硬砂在纺织机械类铸铁件生产中的实际应用,详细阐述了原材料选取,呋喃树脂自硬砂制备工艺、造型与制芯等工序的操作要点及应用实例,分析了呋喃树脂自硬砂代替普通粘土干型砂工艺的利益所在。
3)  Self-solidified furan resin without nitrogen
无氮自硬呋喃树脂
4)  furane resin
呋喃树脂
1.
A study of no-bake furane resin sand technological properties;
自硬呋喃树脂砂工艺性能研究
2.
Through the analysis of the causes of furane FRP internal lining of knock-out drum V209 and laboratory testing of several linings, the acid-resistant ceramic bricks lined with YJ furane resin daub was selected as the internal lining for the drum.
通过对V2 0 9罐“六布八油”呋喃玻璃钢内衬失效原因分析 ,和对几种内衬方案的实验室浸泡试验 ,最后选出用YJ呋喃树脂胶泥贴耐酸瓷砖作为V2 0 9罐内壁的防护
3.
Shell carbon black can be used to modify furane resin for significantly enhancing its electrostatic resistance and impact resistance,so that it is of greater suitability value.
采用谢尔炭黑改性呋喃树脂,能显著提高其抗静电、抗冲击性能,具有较大实用价值。
5)  furan resin
呋喃树脂
1.
Synthesis of furan resin with high strength and weak smell for foundry;
铸造用高强度低气味呋喃树脂合成工艺
2.
Study on novel furan resin with high bonding strength;
高粘结强度新型呋喃树脂的研制
3.
Mechanical properties and applications of furan resin concrete;
呋喃树脂混凝土的力学性能及其应用
6)  furan resin sand
呋喃树脂砂
1.
when producing ductile castings with furan resin sand, the C and S resulted from decomposition of resin and catalyst penetrated into molten iron and caused large quantities of fine flake and dot-shaped supercooling graphites in some areas of the casting which are appearing as dark color defects on the machined surfaces.
采用呋喃树脂砂型铸造球铁件时,由于树脂和硬化剂分解产生的C、S渗入铁液使铸件表层局部区域形成大量密集的细片状和点状过冷石墨,这些区域加工表面上呈灰暗色。
2.
The reason causing nodularization degeneration in surface layer of furan resin sand nodular iron castings was analyzed.
对呋喃树脂砂球墨铸铁件表层球化衰退原因进行了分析。
3.
The variaion pattern of solidification of furan resin sand with the addition of solidifying agents is inquired experimentally and the relationship of proper additive amount of solidifying agents to the temperatures of sand and environment.
通过试验探讨了呋喃树脂砂中固化剂随温度变化的规律 ,得出固化剂的加入量随砂温和环境温度变化的关系式 。