说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 延迟破裂
1)  delayed cracking
延迟破裂
2)  delayed rupture of spleen
延迟性脾破裂
1.
Clinical analysis for traumatic delayed rupture of spleen;
外伤性延迟性脾破裂临床实例分析
2.
Diagnosis and Treatment of Traumatic Delayed Rupture of Spleen:report of 11 cases;
外伤性延迟性脾破裂11例诊断与治疗
3.
Report of 23 cases of delayed rupture of spleen and discussion on nonoperative therapy;
延迟性脾破裂23例报道及其非手术治疗指征的探讨
3)  delayed break
延迟破胶
1.
The delayed break technology was presented.
采用延迟破胶技术,在压裂施工过程中加入不同浓度的胶囊破胶剂,利用它的延缓释放特性,使植物胶压裂液耐温、耐剪切稳定性增强,并且可以在不造成压裂液的流变性、滤失性和携砂性等过早丧失的前提下高浓度使用胶囊破胶剂。
4)  delay-action blasting
延迟爆破
5)  Delayed fracture
延迟破断
6)  delayed fracture
延迟断裂
1.
A Study on Delayed Fracture Resistance of Low Carbon Nb-V Microalloying High Strength Cold Heading Boron Steel
低碳Nb-V微合金化高强度冷镦硼钢耐延迟断裂性的研究
2.
In order to analyze and investigate the effect of heat treatment on delayed fracture resistance of 30MnSi PC steel bars FIP test was adopted.
对30MnSi PC钢棒进行了淬火回火处理,分析探讨了热处理工艺对高强度钢耐延迟断裂性能的影响。
3.
The features and mechanism of fracture of steel bar for prestressed concrete(PC bars) are described,and the material defects which induced the delayed fracture in the PC bars are analyzed in the paper.
介绍了PC钢棒延迟断裂的特征及机理,分析了诱发PC钢棒延迟断裂的材料缺陷。
补充资料:延迟破裂
分子式:
CAS号:

性质:金属材料氢损伤的特征之一。在冶炼、焊接、电镀、酸洗等工序或使用过程中,氢可能进入金属,但并不马上造成破坏,而是积聚在材料内部某些区域,在氢与外加应力的联合作用下经过一段孕育期后,材料内部产生微裂纹,再经过亚临界扩展阶段逐渐长大成临界裂纹,最后导致断裂。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条