Two kinds of wire,core-charged with composite TiAl_3(AW1) and Cr_3C_2(AW2) powder,have been developed,to be used for building up corrosion-resistant coatings of super-critical boiler pipes,by means of supersonic arc-spraying technique.
开发两种适用于超临界锅炉管道防磨的含TiAl3(AW1)、Cr3C2(AW2)的复合粉芯丝材,采用超音速电弧喷涂技术制取耐磨涂层,结合光学显微镜、维氏硬度、X射线衍射、场发射扫描电子显微镜、能谱分析等分析方法对喷涂层的的微观组织结构和高温冲蚀磨损规律进行研究,并与20钢进行对比分析。
4)  boiler tube
锅炉管道
1.
The Boiler Tubes MFL Inspection System Based on LabVIEW
基于LabVIEW的锅炉管道漏磁检测系统
2.
With a view to the shutdown of power plant owing to the crack of the boiler tube by hot corrosion and erosion, the hot corrosion behaviors of FeCrAl/WC composite coating produced by high velocity arc spraying and G20 steel used as the water tube wall material of the power station boiler were investigated.
热腐蚀、冲蚀使火电厂锅炉管道爆裂,致使发电机停机。
3.
To solve the problem of erosion-corrosion wastage at elevated temperature on boiler tube of coal thermal power station, several cored wires for Fe_3Al, Fe_3Al/WC, FeCrAl/WC and FeCrNi/WC intermetallic coatings by high victory arc spraying were developed.
结果表明,温度和攻角对Fe3Al/WC、FeCrAl/WC涂层的冲蚀行为有较大影响;在650℃棱角状石英砂磨粒冲蚀条件下,Fe3Al、Fe3Al/WC、FeCrAl/WC复合涂层的抗冲蚀磨损性能明显优于G20钢,FeCrAl/WC涂层具有最好的全攻角冲蚀磨损抗力,可以作为燃煤锅炉管道的抗高温燃气-飞灰高温冲蚀磨损的防护涂层。
5)  tunnel furnace
隧道炉
6)  tunnel stove
隧道炉
1.
The microcomputer control system for tunnel stove is designed and implemented.
研制了隧道炉微机控制系统 。
补充资料:道-道间寻道时间
道-道间寻道时间(single track seek):  
指磁头从一磁道移动至另一磁道的时间,单位为毫秒(ms)。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条