Aerobic activated sludge in A2/O process possessed better shear stability,and the shear sensitivity(KSS) of their flocs was an order of magnitude less than the anaerobic sludge granules of ABR.
结果表明,厌氧颗粒污泥的剪切敏感性(KSS)比好氧活性污泥高1个数量级,证明了好氧活性污泥的剪切稳定性更好。
3)  adiabatic shear sensitivity
绝热剪切敏感性
1.
In order to reveal the influence of stress state on the adiabatic shear sensitivity, Ti-6Al-4V is heated to get bimodal and lamellar microstructures.
采用分离式Hopkinson压杆技术对双态组织和片层组织Ti-6Al-4V进行了圆柱试样和帽形试样的冲击试验,对比了单轴压缩和压剪复合2种不同应力状态下2种组织钛合金的绝热剪切敏感性差异。
4)  adiabatic shear susceptivity
绝热剪切敏感性
1.
In order to characterise adiabatic shear susceptivity of materials quantitatively, validity in using the parameter Ψ derived from adiabatic shear-band processing energy in evaluating the difference among materials is demonstrated.
采用此测试系统对两种不同组织的新型贝氏体钢进行了绝热剪切敏感性测试,测试结果与前人的认识一致。
2.
Also the relationship between adiabatic shear susceptivity and critical fracture velocity was explored.
利用应力塌陷发生的临界应变作为参量对比了Ti-6Al-4V合金的4种典型组织的绝热剪切敏感性,同时利用Taylor杆实验技术测定了其临界破碎速度,分析了钛合金绝热剪切敏感性与临界破碎速度关系。
3.
The adiabatic shear susceptivity was analyzed quantitatively by the time of flow stress collapse,the uniformly plastic strain before adiabatic shear,the absorbe.
通过对流变应力的塌陷时间 t、绝热剪切前的均匀塑性变形ε、绝热剪切失效前材料所吸收的能量 E 以及绝热剪切带的宽度和密度进行对比分析, 揭示了微观组织对材料绝热剪切敏感性的影响,即随着针状α尺寸的增加材料的绝热剪切敏感性增加。
5)  pseudo-shocks waves
剪切-敏感液晶
6)  Shear Susceptibility
剪切敏性
补充资料:石油产品剪切安定性试验
分子式:
CAS号:

性质:又称石油产品黏度剪切安定性试验(viscosity shear stability test of petroleum products)。矿油型液压油、内燃机油以及黏度添加剂等的使用稳定性质量指标的试验方法。方法有二:(1)机械循环法在标准化设备和规定条件下,将试油连续循环5000次后,测定运动黏度的下降值和酸值的增加值,以百分数表示。(2)超声波照射法。后一方法较前一方法简单,现已被广泛地采用。

说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条