1.
High quality MgO thin films have been successfully grown on glass, Al2O3, Si(111) and Si(100) substrates at 480℃ by using atmospheric-pressure metalorganic chemical vapor deposition (AP-MOCVD)technique.
以2,4-乙酰丙酮化镁为前驱体,衬底温度为480℃,采用MOCVD工艺,分别在玻璃、氧化铝陶瓷、单晶Si(111)和Si(100)衬底上生长了取向生长的氧化镁薄膜。
3)  ZnO thin films
氧化锌薄膜
1.
In this paper, photoluminescence of ZnO thin films, which were deposited by reactive r.
利用直流射频磁控溅射制备了氧化锌薄膜 ,测量了不同温度下的氧化锌薄膜的光致发光 。
2.
The ZnO thin films are fabricated by electrodeposition on n-type InP wafers at constant potential.
采用电化学沉积方法在n型InP(100)(1016)衬底上制备了氧化锌薄膜。
3.
The vacuum evaporation was used for the deposition of Zinc precursor layers,and ZnO thin films were prepared by oxidizing the precursor in the air in the post treatment of annealing processing at different temperatures.
采用真空蒸发镀膜的方法分别在玻璃和硅片衬底上沉积金属锌前驱体,再在空气中通过不同温度的退火氧化处理制得氧化锌薄膜,主要研究了不同退火温度对氧化锌薄膜光电特性的影响。
4)  ZnO film
氧化锌薄膜
1.
Preparation and mechanism of p-type ZnO films formed by modified ion beam enhanced deposition method;
离子束增强沉积制备p型氧化锌薄膜及其机理研究
2.
So it could be used as substrate materials of ZnO films.
ZnWO4单晶的a晶面与氧化锌c晶面晶格匹配很好,是制备氧化锌薄膜的优良衬底。
3.
ZnO films were prepared by pulsed laser deposition on crystal silicon substrate.
在单晶硅衬底上用激光脉冲沉积方法制备了氧化锌薄膜,研究了衬底温度对薄膜结构、形貌和发光性能的影响。
5)  ZnO thin film
氧化锌薄膜
1.
Al-doped ZnO thin films were fabricated on glass substrates by solgel method.
采用溶胶-凝胶工艺在普通玻璃片上制备了掺铝氧化锌薄膜。
2.
N-doped ZnO thin films are grown by plasma-assisted molecular beam epitaxy (P-MBE) on c-plane sapphire (α-Al_2O_3) using NO as oxygen source and nitrogen dopant.
用等离子辅助分子束外延 (P MBE)的方法 ,在蓝宝石c 平面上外延生长了p型氧化锌薄膜。
3.
ZnO thin film was deposited on nucleation side of freestanding diamond film by RF reactive magnetron sputtering.
采用热丝化学气相沉积(CVD)法制备了自支撑金刚石膜,再通过射频磁控溅射法沉积氧化锌薄膜在自支撑金刚石膜上。
6)  zinc oxide film
氧化锌薄膜
1.
A layer of zinc acetate was sprayed on the surface of glass, and then a zinc oxide film as a semiconductor was formed by pyrolysis.
扩展一种和玻璃基体结合力高的化学镀铜技术 ,它在玻璃表面上喷雾覆盖一层醋酸锌 ,然后热解形成半导体氧化锌薄膜 。
补充资料:重质氧化镁 ,氧化镁
药物名称:氧化镁

英文名:Magnesium Oxide

别名: 煅制镁;重质氧化镁 ,氧化镁
外文名:Magnesium Oxide
成分: 由碳酸镁加热而成。有重质和轻质两种一般所指的氧化镁是重质氧化镁。
性状: 为白色粉末;无臭,无味;在空气中能缓缓吸收二氧化碳。在水中几乎不溶,在乙醇中不溶,在稀酸中溶解。
药理作用:
抗酸作用较碳酸氢钠强、缓慢而持久,不产生二氧化碳。与胃酸作用生成氯化镁,放出镁离子,刺激肠道蠕动,具有轻泻作用。
适应症:
适用于伴有便秘的胃酸过多症、胃及十二指肠溃疡病人,对不伴便秘者,其轻泻作用可同服碳酸钙纠正。
用量用法: 抗酸:每次服0.2~1g,1日3次;缓下:每次可服3g,1日3次。
注意事项: 肾功能不全者服用本品可能产生滞留性中毒,如证实为高镁血症可静注钙盐对抗。
药物相互作用: 本品可干扰四环素类的吸收,应避免同时服用。
规格: 片剂:每片0.2g。
氧化镁合剂:由氧化镁60g、重质碳酸镁60g(另加颠茄酊60ml者为复方氧化镁合剂 )


类别:抗酸及抗溃疡药
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条