说明:双击或选中下面任意单词,将显示该词的音标、读音、翻译等;选中中文或多个词,将显示翻译。
您的位置:首页 -> 词典 -> 低倍裂纹
1)  low-multiple crack
低倍裂纹
1.
After researching the character and producing process of low-multiple crack fault in the forged circularity produced by our electric cooker+LF+800ton hydraulic pressure forging equipment,we discussed the influences of craft process on the fault,and process the related measures.
针对我公司电炉+LF+800ton液压锻生产的锻圆出现低倍裂纹缺陷的特征和形成过程进行了深入的研究分析,探讨了生产的各工艺过程对形成低倍裂纹缺陷的影响,并提出了相应措施。
2)  low cyclic fatigue crack
低周疲劳裂纹
1.
In situ observation under SEM is carried out upon the dynamic propagation of low cyclic fatigue cracks in a heat affected zone and a weld metal, which further shows that a certain correlation exists between the growth morphology and pattern and the resistance of the material to the fatigue crack propagation.
在扫描电镜下,对焊接热影响区及一种焊缝金属的低周疲劳裂纹扩展进行了动态原位观察,进一步说明低周疲劳裂纹扩展的形态及方式,以及与材料的疲劳裂纹扩展阻力之间存在着一定的关系,其形态与方式是材料微观组织与特定循环载荷之间相互作用的某种反映。
2.
In situ observation under SEM is carried out for the dynamic propagation of low cyclic fatigue cracks in ferrite pearlite steels.
在扫描电镜下对两种铁素体-珠光体钢中的低周疲劳裂纹扩展进行了动态原位观察,发现疲劳裂纹只在铁素体中扩展,而珠光体晶团阻碍其扩展。
3)  macrostructure [,mækrəu'strʌktʃə]
低倍
1.
According to the macrostructure,decide the reasonable cutting length of the steel.
通过现场跟踪试验,找出了连铸方坯轧制方圆钢产生劈头缺陷的原因,并利用低倍检验确定了合理头尾切除长度,通过现场实践,效果显著,有效解决了连铸方坯轧制方圆钢劈头缺陷问题。
4)  macro [英]['mækrəʊ]  [美]['mækro]
低倍
1.
Design tension cup-type and jaw , develop equipment, adopt macro electrical erosion equipment by analyzing the test for tension and macro-etching of larger round and complete tension and acid macro-etching test.
通过对大规格圆钢的拉伸、低倍检验进行分析,设计制作拉力碗及钳口、并对低倍酸洗方法及设备进行了改进,采用低倍电腐蚀设备,顺利、快捷地完成大规格圆钢试样拉伸试验及低倍酸浸检验,保证了检验工作的正常进行。
5)  low susceptibility to welding crack
低焊接裂纹敏感性
1.
800MPa grade heavy plates with low susceptibility to welding crack produced by direct quenching
直接淬火研制800MPa级低焊接裂纹敏感性高强钢厚板
2.
The microstructure and mechanical properties of 690 MPa grade quench and temper high-strength steel with low susceptibility to welding crack are studied under different temper heat treatment temperatures,and the welding properties of the steel are evaluated by using welding thermal simulation technology.
在不同回火热处理温度下对抗拉强度690 MPa级低焊接裂纹敏感性钢板的力学性能及组织结构进行了研究,并利用焊接热模拟技术对该钢的焊接性能进行了评估。
3.
The strengthening and toughening mechanism of heat affected zone (HAZ) of a high property pressure vessel steel--610MPa grade high heat input welding steel with low susceptibility to welding crack was investigated in this paper by using welding thermal simulation technology.
利用焊接热模拟技术对一种 6 10MPa级大线能量低焊接裂纹敏感性钢的热影响区 (HAZ)强韧化机理进行了研究。
6)  low welding crack sensitivity
低焊接裂纹敏感性
1.
The paper introduces the low welding crack sensitivity steel plate of high input energy welding developed by two iron and steel company.
介绍了中国原油储罐用大线能量用钢的开发和应用现状,并介绍了鞍钢新轧钢股份有限公司和上海宝钢集团公司最近开发的低焊接裂纹敏感性大线能量用钢。
2.
The paper introduces the low welding crack sensitivity steel plate of high input energy welding developed by two iron and steel Co.
本文介绍了我国原油储罐用大线能量用钢的开发和应用现状,介绍了鞍钢新轧钢股份有限公司和上海宝钢集团公司最近开发的低焊接裂纹敏感性大线能量用钢。
补充资料:淬火裂纹和非淬火裂纹的特征及实例分析

淬火裂纹是指在淬火过程中或在淬火后的室温放置过程中产生的裂纹。后者又叫时效裂纹。造成淬火开裂的原因很多,在分析淬火裂纹时,应根据裂纹特征加以区分。


一、淬火裂纹的特征


在淬火过程中,当淬火产生的巨大应力大于材料本身的强度时,便会导致裂纹产生。淬火裂纹往往是在马氏体转变开始进行后不久产生的,裂纹的分布则没有一定的规律,但一般容易在工件的棱角槽口、截面突变处形成。


在显微镜下观察到的淬火开裂,可能是沿晶开裂,也可能是穿晶开裂;有的呈放射状,也有的呈单独线条状或呈网状。


因在马氏体转变区的冷却过快而引起的淬火裂纹,往往是穿晶分布,而且裂纹较直,周围没有分枝的小裂纹。


因淬火加热温度过高而引起的淬火裂纹,都是沿晶分布,裂纹尾端尖细,并呈现过热特征:结构钢中可观察到粗针状马氏体;工具钢中可观察到共晶或角状碳化物。


表面脱碳的高碳钢工件,淬火后容易形成网状裂纹。这是因为,表面脱碳层在淬火冷却时的体积胀大比未脱碳的心部小,表面材料受心部膨胀的作用而被拉裂呈网状。


二、非淬火裂纹的特征


淬火后发生的裂纹,不一定都是淬火所造成的,一般可根据下面的特征来区分。


淬火后发现的裂纹,如果裂纹两侧有氧化脱碳现象,则可以肯定裂纹在淬火之前就已经存在。淬火冷却过程中,只有当马氏体转变量达到一定数量时,裂纹才有可能形成。与此相对应的温度,大约在250℃以下。在这样的低温下,即使产生了裂纹,裂纹两侧也不会发生脱碳和出现明显氧化。所以,有氧化脱碳现象的裂纹是非淬火裂纹。


如果裂纹在淬火前已经存在,又不与表面相通,这样的内部裂纹虽不会产生氧化脱碳,但裂纹的线条显得柔软,尾端圆秃,也容易与淬火裂纹的线条刚健有力,尾端尖细的特征区别开来。


三、实例分析


实例一:


40Cr钢制成的转子轴,经锻造、淬火后发现裂纹。裂纹两侧有氧化迹象,经金相检验,裂纹两侧存在脱碳层,而且裂纹两侧的铁素体呈较大的柱状晶粒,其晶界与裂纹大致垂直。结论:裂纹是在锻造时形成的非淬火裂纹。


当工件在锻造过程中形成裂纹时,淬火加热即引起裂纹两侧氧化脱碳。随着脱碳过程的进行,裂纹两侧的碳含量降低,铁索体晶粒开始生核。当沿裂纹两侧生核的铁素体晶粒长大到彼此接触后,便向离裂纹两侧较远的基体方向生长。由于裂纹两侧在脱碳过程中碳浓度的下降,也是由裂纹的开口部位向内部发展,因而为铁素体晶粒的不断长大提供了条件,故最终长大为晶界与裂纹相垂直的柱状晶体。


说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条