1) tetrabromo-bisphenol-A epoxy resin
四溴双酚A环氧树脂
1.
By means of fourier transform infrared(FTIR), the curing kinetics of bisphenol-S epoxy resin/DDS and tetrabromo-bisphenol-A epoxy resin/DDS at constant temperature were studied, and the apparent activation energy was obtained.
用傅里叶红外光谱 (FTIR)法研究了双酚S环氧树脂和四溴双酚A环氧树脂分别与二胺基二苯砜在恒温条件下的固化反应动力学 ,得出了各反应的表观活化能。
2) brominated bisphenol A epoxy resin
溴代双酚A环氧树脂
3) Bromine-containing naphthol formaldehyde epoxy resin
含溴萘酚酚醛环氧树脂
4) bisphenol A epoxy resin
双酚A型环氧树脂
1.
The effects of curing temperature and the content of on the curing speed of PSN-1 polysilazane/bisphenol A epoxy resin curing system were discussed.
研究了聚硅氮烷(PSN-1)/双酚A型环氧树脂固化体系的固化温度、PSN-1用量对固化速度的影响;并利用热重分析(TGA)研究了PSN-1用量对固化树脂高温残余质量分数的影响,对固化机理进行了初步探讨。
5) bisphenol A epoxy resin
双酚A环氧树脂
1.
Describe the production prenciple,raw material and process of bisphenol A epoxy resin.
描述了双酚A环氧树脂生产的反应机理 ,原材料 ,主要建筑用胶的性能和特点及质量参
补充资料:2,2',6,6'-四溴双酚A
分子式:C15H12Br4O2
分子量:543.90
CAS号:79-94-7
性质:灰白色粉末。熔点180-184℃,沸点316℃(分解)。溶于甲醇和乙醚,不溶于水。
制备方法:双酚在室温下加溴,通氯,经溴化反应、过滤、水洗、干燥,得成品。原料消耗定额:双酚 A 840kg/t、溴素350kg/t、液氯(98%)800kg/t。
用途:用于塑料、橡胶、纺织、纤维和造纸等工业作阻燃剂,如用于环氧、聚碳酸酯、聚酯、酚醛及ABS等树脂中,使制品具有良好的阻燃性和自熄性。目前正式用于电视高压包灌注环氧树脂中。
分子量:543.90
CAS号:79-94-7
性质:灰白色粉末。熔点180-184℃,沸点316℃(分解)。溶于甲醇和乙醚,不溶于水。
制备方法:双酚在室温下加溴,通氯,经溴化反应、过滤、水洗、干燥,得成品。原料消耗定额:双酚 A 840kg/t、溴素350kg/t、液氯(98%)800kg/t。
用途:用于塑料、橡胶、纺织、纤维和造纸等工业作阻燃剂,如用于环氧、聚碳酸酯、聚酯、酚醛及ABS等树脂中,使制品具有良好的阻燃性和自熄性。目前正式用于电视高压包灌注环氧树脂中。
说明:补充资料仅用于学习参考,请勿用于其它任何用途。
参考词条