1)  microetch
微蚀量
2)  microetch
微蚀
1.
The influences of microetch,temperature and pH on deposit were discussed,and hence some suitable process conditions were obtained as follows: an optimum microetch solution of a mixed solution with the volume ratio of hydrogen peroxide to sulfuric acid being 1∶4,an optimum temperature 85~90 ℃ an.
通过讨论温度、pH对镀层的影响,确定最佳微蚀液为双氧水与硫酸的体积比为1∶4的混合液,镀镍与镀金最佳温度都为85~90℃,最佳pH分别为4。
2.
Introduce one-step microetch cleaner ST-10 for photoresist adhesion and it s performances.
介绍同时具有除油、微蚀和防氧化三重功效的一步法干膜前处理液ST-10的组成、工艺及其性能。
3.
The factors which affect hydrogen peroxide s decomposition and the mechanism of hydro-gen peroxide s stabilization in microetchant has been described.
分析微蚀液中影响H_2O_2分解的因素,探讨其稳定机理。
3)  Micro-etch
微蚀刻
1.
Comparative Study on Potassium Monopersulfate Compound and Sodium Persulfate in the PCB Micro-etch Field;
过硫酸氢钾复合盐与过硫酸钠在PCB微蚀刻中的对比研究
4)  micro-etching holes
微蚀孔
1.
In this case,it is likely that some micro-etching holes can be found on the surface of the film.
分析可知,微蚀孔并不完全在第2次腐蚀的过程中形成,而是从第1次深腐蚀过程中对掩膜层的钻蚀开始的。
5)  microetchant
微蚀液
1.
Research on microetchant for black oxide pretreatment of PCB lining;
印制线路板内层黑氧化前处理微蚀液的研制
6)  microetching rate
微蚀速率